Plenary Speakers

  • Professor

    Erik Bitzek

    Max-Planck-Institut für Eisenforschung GmbH, DE

    "Atomistic Simulations of Dislocation – Precipitate Interactions in Model Ni-based Superalloys"

  • Professor

    Nathalie Bozzolo

    CEMEF, Centre de Mise en Forme des Matériaux, Mines Paris, Sophia Antipolis, FR

    "Recrystallization and grain size control in γ- γ’ Ni based superalloy forgings"

  • PhD

    Mark Hardy

    Rolls-Royce plc, UK

    "Forging and heat treatment conditions that produce visible grains in a nickel alloy"

  • Professor

    Catherine Rae

    Rolls-Royce UTC, UK

    "Tensile Deformation in Single Crystal Superalloys: The Effect of Strain Rate"

  • Assistant professor

    Jean-Charles Stinville

    University of Illinois at Urbana-Champaign, US

    "Plastic localization and Fatigue Strength in Polycrystalline Nickel-Based Superalloys"

  • PhD

    Satoshi Utada

    University of Oxford, Department of Materials, UK

    "Detecting phase transition temperature and microstructure evolution behaviors of Ni-based superalloys using resistivity and calorimetry"

  • Dr.

    Jian Zhang

    Institute of Metal Research, Chinese Academy of Sciences, CN

    "Recrystallization in Ni-based single crystal superalloys"

Superalloys 2022
18 - 22 September 2022 | Hybrid Symposium in Bamberg (Germany) & Online